Cladding render brickwork

Wall sarking installation defects

3 examples in 2 videos 1 major 2 minor

What it is

The pliable building membrane behind the wall does not have the mandatory 150 mm overlap or taped seams, compromising weather and fire barrier integrity.

Wall sarking was left unengaged and does not extend into the bottom starter strip as required by the manufacturer's manual, allowing water ingress behind the cladding system.

Non-breathable reflective foil was installed hard against framing without drainage cavity battens, trapping condensation and causing rot behind polystyrene cladding.

Standards