Plasterboard lining installation defects and clearances
What it is
Non-compliant ductwork and missing back blocking were identified within the home. In addition, internal plasterboard corners exhibit cracking and substandard silicone patch repairs.
Internal wall plasterboard sheets were fitted hard down against the concrete floor without the required 6 mm to 10 mm expansion clearance. Ground contact exposes the plaster to edge cracking upon structural deflection or moisture absorption.
Standards
- AS/NZS 2589 Suggested reference, unverified
Explained in our own words. Check the current edition; which edition applies depends on the building permit date.
Also relevant to
Video examples
- I Uncovered a First Home Buyer’s Worst Nightmare 3:01 minorDefective internal lining finishes, ductwork, and back blocking
- The Shocking Truth: Builder Vanishes, Leaving Half-Finished Project... 25:41 minorInternal plasterboard sheets installed tight against floor substrate