What it is

Fastener penetrations through the sheeting were left open without required seals or gaskets. These unsealed openings permit water ingress directly into the roof cavity.

Roof fixing screws across the metal roof sheets were overtightened during installation. Compressing the rubber neoprene washers beyond manufacturer limits has damaged weather seals and compromised roof watertightness.

Roof fasteners are installed further apart than permitted, exceeding the maximum allowed distance of 100 mm. Improper fastening increases the risk of sheet detachment and water ingress.