Membrane application thickness and integrity defects
What it is
The applied waterproofing membrane is visibly under-gauge, failing to achieve the manufacturer-specified minimum dry film thickness of 1 mm. Exposed base coat and substrate paper demonstrate inadequate coverage.
The liquid-applied waterproofing membrane exhibits visible pinholes and was coated over an unprepared surface before prior work was properly finished. These pinholes compromise the continuous seal and permit water penetration.
Paint was applied directly over the waterproofing membrane in areas intended for tiling. This violates manufacturer instructions and prevents tile adhesive from bonding properly to the substrate.
Standards
- AS 3740 Suggested reference, unverified
Explained in our own words. Check the current edition; which edition applies depends on the building permit date.
Also relevant to
Video examples
- I Caught This Waterproofing Contractor On Bodycam… 1:11 majorInsufficient dry film thickness of waterproofing membrane
- I Caught This Waterproofing Contractor On Bodycam… 2:33 majorPinholes in applied waterproofing membrane
- Uncovering the Secrets: Confronting Supervisor over Leaks | BodyCam Footage 0:55 majorPaint applied over waterproofing membrane