Missing or defective bond breakers and fillet joints
What it is
The external Class 3 liquid membrane lacks proper horizontal-to-vertical bond breaker transitions, creating severe stress pinholes. The membrane was also applied straight onto raw render without required termination protection.
The external terrace membrane lacks required 15 mm by 15 mm polyurethane or tape bond breakers at horizontal-to-vertical perimeter junctions. The membrane is cracking across junctions due to unrestrained thermal movement.
External membrane transition from horizontal to vertical lacks a 15x15 mm bond breaker fillet, resulting in split cracking and ruptured waterproofing.
Standards
Explained in our own words. Check the current edition; which edition applies depends on the building permit date.
Also relevant to
Video examples
- Unveiling Worst Builder of 2023 55:46 majorDefective membrane bond breaker and pinholing at perimeter junctions
- I Inspected a Billionaire’s Mansion 1:03:47 majorMissing 15x15mm bond breakers causing bridging cracks in membrane
- I inspected a $20 Million Government Housing Build 24:08 majorAbsence of bond breaker fillet causing membrane bridging splits